| 141 |
|
Fracture behaviour of liquid crystal epoxy resin systems based on the diglycidyl ether of 4,4'-dihydroxy-�methylstilbene and sulphanilamide Part1 Effects of curing variations
|
Sue, H. J. Earls, J. D. Hefner, R. E.
|
Chapman and Hall
|
1997
|
|
|
|
| 142 |
|
Fracture behaviour of SiC fibre-reinforced nitrogen glass matrix composites
|
Thompson, D. P. Zhang, E.
|
Chapman and Hall
|
1996
|
|
|
|
| 143 |
|
Fracture behaviour of virgin and recycled isotactic polypropylene/
|
Urrutibeascoa, I; Aurrekoetxea, J Sarrionandia, M A; Maspoch, M Li
|
Chapman and Hall
|
2001
|
|
|
|
| 144 |
|
Fracture chemistry of �Al~2O~3 (Saffil) fibres in an MgLi matrix environment
|
Gergely, V. Kudela, S. Baunack, S. John, A.
|
Chapman and Hall
|
1997
|
|
|
|
| 145 |
|
Fracture in potato tuber parenchyma
|
Hiller, S
|
Chapman and Hall
|
1996
|
|
|
|
| 146 |
|
Fracture lances in glass loaded with spherical indenters/
|
Momber, A. W.
|
Chapman and Hall
|
2003
|
|
|
|
| 147 |
|
Fracture mechanics behaviour of austenitic compacted graphite cast iron
|
Hsu, C.-H
|
Chapman and Hall
|
1996
|
|
|
|
| 148 |
|
Fracture mechanics of oilseed rape pods
|
Davies, G. C
|
Chapman and Hall
|
1997
|
|
|
|
| 149 |
|
Fracture mechanics of single-fibre pull-out test
|
Wang, C.
|
Chapman and Hall
|
1997
|
|
|
|
| 150 |
|
Fracture mechanism of NCG reinforced MMC fabricated by the squeeze casting method/
|
Ryu, Y M Rhee, M H Yoon, E P;
|
Chapman and Hall
|
2000
|
|
|
|
| 151 |
|
Fracture mechanisms in a stoichiometric 3Al~2O~32SiO~2 mullite
|
Baudin, C.
|
Chapman and Hall
|
1997
|
|
|
|
| 152 |
|
Fracture mechanisms of poly(ethylene terephthalate) and blends with styrene-butadiene-styrene elastomers
|
Moet, A. Tanrattanakul, V. Perkins, W. G. Massey, F. L.
|
Chapman and Hall
|
1997
|
|
|
|
| 153 |
|
Fracture mechanisms of the Strombus gigas conch shell: implications for the design of brittle laminates
|
Kessler, H. Kuhn-Spearing, L. T. Ballarini, R. Chateau, E.
|
Chapman and Hall
|
1996
|
|
|
|
| 154 |
|
Fracture mode for self-fragmentation of carbon contaminated icosahedral Al-Cu-Fe quasicrystalline phase/
|
|
Chapman and Hall
|
2001
|
|
|
|
| 155 |
|
Fracture of brittle multiphase materials by high energy water jets
|
Momber, A
|
Chapman and Hall
|
1996
|
|
|
|
| 156 |
|
Fracture process of thermally shocked discontinuous fibre-reinforced glass matrix composites under tensile loading
|
Prewo, K. M. Ogi, K. Takeda, N.
|
Chapman and Hall
|
1997
|
|
|
|
| 157 |
|
Fracture resistance of polyblends and polyblend matrix composites. Part II. Role of the rubber phase in nylon 6,6/ABS alloys
|
Goettler, L. A. Nair, S. V. Subramaniam, A.
|
Chapman and Hall
|
1997
|
|
|
|
| 158 |
|
Fracture resistance of polyblends and polyblend matrix composites. Part I. Unreinforced and fibre-reinforced nylon 6,6/ABS polyblends
|
Wong, S.-C. Goettler, L. A. Nair, S. V.
|
Chapman and Hall
|
1997
|
|
|
|
| 159 |
|
Fracture strength and toughness of some phenolic concretes
|
Shariatmadari, A. A
|
Chapman and Hall
|
1996
|
|
|
|
| 160 |
|
Fracture toughness and crack morphology in indentation fracture of brittle materials
|
Tanaka, M
|
Chapman and Hall
|
1996
|
|
|
|